Nanostructured copper alloy rivals superalloys in strength and stability - Phys.org
Lehigh University |
Technology |
Phys.Org |
03-29-2025 |
26
Researchers from the U.S. Army Research Laboratory (ARL) and Lehigh University have developed a nanostructured copper alloy that could redefine high-temperature materials for aerospace, defense, and …